Non-toxic EVA Plastic used in Shoe making industry
SPECIFICATIONS:
| EVA UE1803 | ||
| ITEM | Specifications | RESULTS OF ANALYSIS |
| Black grain,PCS/KG | 0 | 0 |
| Color grain,PCS/KG | ≤10 | 0 |
| Big and small grain ,PCS/KG | ≤10 | 0 |
| Trailing grain,PCS/KG | ≤20 | 2 |
| Floccule,g/kg | ≤0.02 | 0 |
| VA,%(wt) | 18(+/-)1 | 17.3 |
| Melt mass flow rate,g/10min | 2.8(+/-)0.5 | 3.17 |
| Density,(23 ºC)g/m3 | As report | 0.937 |
| Melting peak temperature,ºC | As report | 90 |
| EVA UE2825 | |
| ITEM | Specification |
| Black grain,PCS/KG | 0 |
| Color grain,PCS/KG | ≤7 |
| Snakeskin grain,PCS/KG | ≤1 |
| Trailing grain,PCS/KG | As report |
| Floccule,g/kg | ≤0.5 |
| VA,%(wt) | 27.5(+/-)1 |
| Tensile break stress,Mpa | ≥6 |
| Yellow index | ≤2 |
| Melt mass flow rate,g/10min | 25(+/-)2.5 |
| Tensile fracture nominal strain,% | ≥600 |
EVA 28%
| PROPERTIES | TEST METHOD | UNIT | Data |
| VA Content | % | 28.0 | |
| Density | ASTM D1505 | g/cm3 | 0.954 |
| Melt Index MI2.16 | ASTM D1238 | g/10min | 15 |
| Tensile Strength (Break) | ASTM D638 | Kg/cm2 | 80 |
| Elongation at break | ASTM D638 | % | >800 |
| Melting point | ASTM D-3418 | ºC | 69 |
| Hardness | ASTM D2240 | Shore D | 20 |
1) Processing grade: extrusion grade, injection grade, hot melt grade.
1.We are able to provide customized service based on your requirements.
2. Competitive prices - directly from factory to customer.
3.Advanced equipments for testing and manufacturing.
4.Professional and good after-sale service
5. Free sample for testing