Standard & Material | Acero al carbono | La norma ASTM A519 | MT1010, MT1020, 1008, 1010, 1018 y 1020, 1025, 1030, 1045, 1518 |
La norma JIS G3445 | STKM STKM11A12A 12B STKM STKM STKM12C13A 13B STKM STKM STKM13C14A STKM STKM14B14C 15A STKM STKM STKM15C16A 16C STKM STKM STKM17A17C 18A STKM STKM STKM18B18C 19A STKM STKM STKM19C20A | ||
La norma JIS G3473 | STC370, STC440, STC510A, STC510, STC540, STC590A, B590STC. | ||
La norma DIN 2391 | St 35, ST45, ST52 | ||
La norma EN 10297-1 Standard | E235, E275, E315, E355, E470 | ||
La norma EN 10305-1 Standard | E215, E235 E355 | ||
La norma EN 10305-4 Standard | E215, E235 E355 | ||
La norma BS 6323-3 | HFS HFS 3, 4, 5, 8 de HFS HFS | ||
A49-311 NF | TU 37-b, TU 52-b, TU 56-b, TU XC35 | ||
Aleación de acero, | La norma ASTM A519 | 1345, 3140, 4130, 4135, 4140, 4150, 4320, 4340, 5120, 5130 | |
La norma JIS G3429 | STH11, 12 STH21, 122 STH31 | ||
La norma JIS G3441 | SCR420TK, SCM415TK, SCM418TK, SCM420TK, SCM430TK, SCM440TK | ||
Acero inoxidable | La norma ASTM A511 | MT304, MT304L, MT310S, MT316, MT316L, MT317, MT321, MT347, MT403, MT410 MT431 | |
La norma ISO | NACE El Sr. -0175 | ||
El tamaño |
La gama de tamaños | La tolerancia | |
OD. | 6-325mm | -- +0.045-0.035 mm | |
ID. | 2-250mm | ± 0.035mm | |
WT | 1-32mm | Depende de tallas | |
Longitud | Azar o de longitud fija | +0-3.5mm | |
La rectitud | 0.15: 1000: 1000, 0.4, 0.5: 1000 1: 1000 o personalizado | ||
La rugosidad superficial | Ra 0.02-0.4μm |
Grado de acero | C(%) | Si(%) | Mn(%) | P(%) | S(%) | Nb/V(%) |
STKM11A | ≤0, 12 | ≤0, 35 | ≤0, 60 | ≤ 0.040 | ≤ 0.040 | - |
STKM12A | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤ 0.040 | ≤ 0.040 | - |
STKM12B | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤ 0.040 | ≤ 0.040 | - |
STKM12C | ≤0, 20 | ≤0, 35 | ≤0, 60 | ≤ 0.040 | ≤ 0.040 | - |
STKM13A | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤ 0.040 | ≤ 0.040 | - |
STKM13B | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤ 0.040 | ≤ 0.040 | - |
STKM13C | ≤0, 25 | ≤0, 35 | 0.30~0.90 | ≤ 0.040 | ≤ 0.040 | - |
STKM14A | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤ 0.040 | ≤ 0.040 | - |
STKM14B | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤ 0.040 | ≤ 0.040 | - |
STKM14C | ≤0, 30 | ≤0, 35 | 0.30~1.00 | ≤ 0.040 | ≤ 0.040 | - |
STKM15A | 0.25~0.35 | ≤0, 35 | 0.30~1.00 | ≤ 0.040 | ≤ 0.040 | - |
STKM15C | 0.25~0.35 | ≤0, 35 | 0.30~1.00 | ≤ 0.040 | ≤ 0.040 | - |
Grado de acero | Fuerza tensil(N/mm²) | Límite de fluencia(N/mm²) |
STKM11A | ≥290 | - |
STKM12A | ≥340 | ≥175 |
STKM12B | ≥390 | ≥275 |
STKM12C | ≥470 | ≥355 |
STKM13A | ≥370 | ≥215 |
STKM13B | ≥440 | ≥305 |
STKM13C | ≥510 | ≥380 |
STKM14A | ≥410 | ≥245 |
STKM14B | ≥500 | ≥355 |
STKM14C | ≥550 | ≥410 |
STKM15A | ≥470 | ≥275 |
STKM15C | ≥580 | ≥430 |
+C (BK) | El frío atraído/disco. Después de la última formación de frío, sin tratamiento térmico. |
+LC(BKW) | El frío atraído/soft. Después del último tratamiento térmico sigue el dibujo de frío hay una luz pase de acabado. |
+SR(BKS) | Alivia el estrés de frío y recocidos. Después del último proceso de estirado en frío los tubos se alivia el estrés en el recocido atmósfera controlada. |
+Una(GBK) | Después del último proceso de estirado en frío los tubos se alivia el estrés en el recocido atmósfera controlada. |
+N(NBK) | Normalizado. Después del último proceso de estirado en frío los tubos son recocido en una atmósfera controlada. |