Koperlegering | Chemische samenstelling | Temper | Mechanische eigenschappen |
Korrelgrootte
mm |
||
Koper
% |
Fosfor
% |
Treksterkte
MPa |
Verlenging
% |
|||
C12200 | ≥ 99.90 | 0.015-0.040 | O60 | ≥ 205 | ≥ 40 | ≥ 0.040 |
C12200 | ≥ 99.90 | 0.015-0.040 | O50 | ≥ 205 | ≥ 40 | 0.015-0.040 |
Koperlegering | Chemische samenstelling | Temper | Mechanische eigenschappen | |||
Koper
% |
Fosfor
% |
Treksterkte
MPa |
Verlenging
% |
Hardheid
HV |
||
Cu-DHP | ≥ 99.90 | 0.015-0.040 | R220 | ≥ 220 | ≥ 40 | 40-70 |
Koperlegering | Chemische samenstelling | Temper |
Hardheid
HV |
Korrelgrootte
mm |
|
Koper
% |
Fosfor
% |
||||
C12200 | ≥ 99.90 | 0.015-0.040 | O | ≤ 75 | ≤ 0.065 |
Koperlegering | Temper | Reinheid | Standaard |
C12200 | O60 | ≤ 38 mg/m² |
ASTM B280 / ASTM B68 / ASTM B743 /
EN 12735-1 / AS 1571 |
koperen buis met vlakke gewikkelde spoel (mm) | |||||||||||
W. T.
O. D. |
≥0.28- 0.41 | ≥0.41- 0.50 | ≥0.50- 0.61 | ≥0.61- 0.71 | ≥0.71- 0.81 | ≥0.81- 0.91 | ≥0.91- 1.02 | ≥1.02- 1.22 | ≥1.22- 1.50 | ≥1.50- 1.65 | ≥1.65 |
4 | √ | √ | √ | √ | |||||||
4.76 (16 inch) | √ | √ | √ | √ | √ | ||||||
5 | √ | √ | √ | √ | √ | √ | |||||
6 | √ | √ | √ | √ | √ | √ | √ | ||||
6.35 (1/4") | √ | √ | √ | √ | √ | √ | √ | √ | |||
7 | √ | √ | √ | √ | √ | √ | √ | √ | |||
7.94 (5/16") | √ | √ | √ | √ | √ | √ | √ | √ | √ | ||
8 | √ | √ | √ | √ | √ | √ | √ | √ | √ | ||
9 | √ | √ | √ | √ | √ | √ | √ | √ | √ | ||
9.52 (3/8") | √ | √ | √ | √ | √ | √ | √ | √ | √ | ||
10 | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ |
12 | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ |
12.7 (1/2") | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ |
15 | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | |
15.88 (5/8") | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | |
16 | √ | √ | √ | √ | √ | √ | √ | √ | √ | √ | |
18 | √ | √ | √ | √ | √ | √ | √ | √ | |||
19.05 (3/4") | √ | √ | √ | √ | √ | √ | √ | √ | |||
20 | √ | √ | √ | √ | √ | √ | √ | √ | |||
22 | √ | √ | √ | √ | √ | √ | |||||
22.23 (7/8") | √ | √ | √ | √ | √ | √ |