Grondstoffen | ||||
HRC | Metrical | MG korrelgrootte (μm) | CO(%) | Flexural Strength (N/mm²) |
45° | ZK30 | 0.7 | 10 | 3320 |
50° | CB WF25 | 0.6 | 10 | 4000 |
55° | K44UF Gurhing | 0.5 | 12 | 4300 |
65° | CTU08L CERATIZIT | 0.4 | 10 | 3700 |
Supercoating | ||||
Altin | TiAIN | TiSiN | Nano | |
Hardheid (HV) | 3200 | 2800 | 3600 | 42 (GPA) |
Dikte (μm) | 2.5-3 | 2.5-3 | 3 | 3 |
Oxidatietemperatuur (ºC) | 900 | 800 | 1000 | 1200 |
Wrijvingscoëfficiënt | 0.3 | 0.3 | 0.45 | 0.4 |
Kleur | Zwart | Paars | Koper | Blauw |